General
Property | Value | Shape | Related Standards |
---|---|---|---|
Density | 4.37 g/cm³ Show Material materials with Density of 4.37 g/cm³ | Bar, Billet | |
4.37 g/cm³ Show Material materials with Density of 4.37 g/cm³ | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Dimension
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Diameter | 7 mm Show Material materials with Diameter of 7 mm | Bar | ||
115 mm Show Material materials with Diameter of 115 mm | Bar | |||
130 mm Show Material materials with Diameter of 130 mm | Billet | |||
350 mm Show Material materials with Diameter of 350 mm | Billet | |||
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Length | 3000 mm Show Material materials with Length of 3000 mm | Billet | ||
4500 mm Show Material materials with Length of 4500 mm | Billet | |||
6000 mm Show Material materials with Length of 6000 mm | Bar | max |
Mechanical
Property | Value | Shape | Related Standards |
---|---|---|---|
Elastic modulus | 117.0 GPa Show Material materials with Elastic modulus of 117.0 GPa | Bar, Billet | |
128 GPa Show Material materials with Elastic modulus of 128 GPa | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Elongation | 10.0 % Show Material materials with Elongation of 10.0 % | Bar, Billet | |
Hardness, Rockwell C | 36.0 [-] Show Material materials with Hardness, Rockwell C of 36.0 [-] | Bar, Billet | |
Impact strength, Charpy notched | 20.0 - 34.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 20.0 - 34.0 kJ/m² | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | |
Poisson's ratio | 0.35 [-] Show Material materials with Poisson's ratio of 0.35 [-] | Bar, Billet | |
Shear modulus | 42.0 GPa Show Material materials with Shear modulus of 42.0 GPa | Bar, Billet | |
Tensile strength | 897.0 MPa Show Material materials with Tensile strength of 897.0 MPa | Bar, Billet | |
931.0 MPa Show Material materials with Tensile strength of 931.0 MPa | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Yield strength | 827.0 MPa Show Material materials with Yield strength of 827.0 MPa | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Thermal
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 0.0000085 1/K Show Material materials with Coefficient of thermal expansion of 0.0000085 1/K | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | |
20 °C | 0.0000090 1/K Show Material materials with Coefficient of thermal expansion of 0.0000090 1/K | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
100 °C | 0.0000085 1/K Show Material materials with Coefficient of thermal expansion of 0.0000085 1/K | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
315 °C | 0.0000090 1/K Show Material materials with Coefficient of thermal expansion of 0.0000090 1/K | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Melting point | 1538.0 °C Show Material materials with Melting point of 1538.0 °C | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Specific heat capacity | 502 J/(kg·K) Show Material materials with Specific heat capacity of 502 J/(kg·K) | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Thermal conductivity | 6 W/(m·K) Show Material materials with Thermal conductivity of 6 W/(m·K) | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
6.5 W/(m·K) Show Material materials with Thermal conductivity of 6.5 W/(m·K) | Bar, Billet |
Electrical
Property | Value | Related Standards |
---|---|---|
Electrical resistivity | 1.9699999999999998e-06 Ω·m Show Material materials with Electrical resistivity of 1.9699999999999998e-06 Ω·m | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Chemical properties
Property | Value | Shape | Related Standards |
---|---|---|---|
Aluminium | 7.35 - 8.35 % Show Material materials with Aluminium of 7.35 - 8.35 % | Bar, Billet | |
7.5 - 8.5 % Show Material materials with Aluminium of 7.5 - 8.5 % | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Carbon | 0.08 Show Material materials with Carbon of 0.08 | Bar, Billet | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Hydrogen | 0.0125 Show Material materials with Hydrogen of 0.0125 | Bar, Billet | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Iron | 0.3 Show Material materials with Iron of 0.3 | Bar, Billet | |
Molybdenum | 0.75 - 1.25 % Show Material materials with Molybdenum of 0.75 - 1.25 % | Bar, Billet | |
0.75 - 1.75 % Show Material materials with Molybdenum of 0.75 - 1.75 % | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 | ||
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | Bar, Billet | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Oxygen | 0.12 Show Material materials with Oxygen of 0.12 | Bar, Billet | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |
Vanadium | 0.75 - 1.75 % Show Material materials with Vanadium of 0.75 - 1.75 % | Bar, Billet | AMS 4915, AMS 4916, AMS 4972, AMS 4973, MIL-T 9046, MIL-T 9047 |