General
Property | Value | Related Standards | Shape |
---|---|---|---|
Density | 4.51 g/cm³ Show Material materials with Density of 4.51 g/cm³ | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Dimension
Property | Value | Related Standards | Shape |
---|---|---|---|
Diameter | 5 mm Show Material materials with Diameter of 5 mm | ASTM B-265, DIN 17860 | Tube |
12.7 mm Show Material materials with Diameter of 12.7 mm | ASTM B-265, DIN 17860 | Tube | |
25.4 mm Show Material materials with Diameter of 25.4 mm | ASTM B-265, DIN 17860 | Billet | |
38.1 mm Show Material materials with Diameter of 38.1 mm | ASTM B-265, DIN 17860 | Tube | |
125 mm Show Material materials with Diameter of 125 mm | ASTM B-265, DIN 17860 | Billet | |
130 mm Show Material materials with Diameter of 130 mm | ASTM B-265, DIN 17860 | Tube | |
Length | 1000 mm Show Material materials with Length of 1000 mm | ASTM B-265, DIN 17860 | Tube |
1500 mm Show Material materials with Length of 1500 mm | ASTM B-265, DIN 17860 | Sheet, Plate | |
5000 mm Show Material materials with Length of 5000 mm | ASTM B-265, DIN 17860 | Sheet, Tube | |
6500 mm Show Material materials with Length of 6500 mm | ASTM B-265, DIN 17860 | Plate | |
20000 mm Show Material materials with Length of 20000 mm | ASTM B-265, DIN 17860 | Tube | |
Wall thickness | 0.4 - 1.65 mm Show Material materials with Wall thickness of 0.4 - 1.65 mm | ASTM B-265, DIN 17860 | Tube |
0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | ASTM B-265, DIN 17860 | Tube | |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | ASTM B-265, DIN 17860 | Billet | |
Width | 400 mm Show Material materials with Width of 400 mm | ASTM B-265, DIN 17860 | Sheet |
600 mm Show Material materials with Width of 600 mm | ASTM B-265, DIN 17860 | Plate | |
1524 mm Show Material materials with Width of 1524 mm | ASTM B-265, DIN 17860 | Sheet | |
1600 mm Show Material materials with Width of 1600 mm | ASTM B-265, DIN 17860 | Plate |
valueMetaData
Property | Value |
---|
Mechanical
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastic modulus | 105.0 GPa Show Material materials with Elastic modulus of 105.0 GPa | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Elongation | 20.0 % Show Material materials with Elongation of 20.0 % | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Hardness, Brinell | 150.0 Show Material materials with Hardness, Brinell of 150.0 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Poisson's ratio | 0.361 [-] Show Material materials with Poisson's ratio of 0.361 [-] | Typical for Pure Titanium | ||
Shear modulus | 46.0 GPa Show Material materials with Shear modulus of 46.0 GPa | Typical for Pure Titanium | ||
Tensile strength | 345.0 MPa Show Material materials with Tensile strength of 345.0 MPa | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Yield strength | 275.0 MPa Show Material materials with Yield strength of 275.0 MPa | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Thermal
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | ||
Melting point | 1670.0 °C Show Material materials with Melting point of 1670.0 °C | Typical for Pure Titanium | ||
Specific heat capacity | 520 J/(kg·K) Show Material materials with Specific heat capacity of 520 J/(kg·K) | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube | |
Thermal conductivity | 20 W/(m·K) Show Material materials with Thermal conductivity of 20 W/(m·K) | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Carbon | 0.08 Show Material materials with Carbon of 0.08 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Hydrogen | 0.015 Show Material materials with Hydrogen of 0.015 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Iron | 0.3 Show Material materials with Iron of 0.3 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Nitrogen | 0.03 Show Material materials with Nitrogen of 0.03 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |
Oxygen | 0.25 Show Material materials with Oxygen of 0.25 | ASTM B-265, DIN 17860 | Sheet, Plate, Billet, Tube |