GOST PT1M

Want to keep this datasheet? Save it now in your required format

This material data has been provided by VSMPO,Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueShape

Density

4.49 g/cm³

Show Material materials with Density of 4.49 g/cm³

Tube

Dimension

PropertyValueShape

Diameter

5 mm

Show Material materials with Diameter of 5 mm

Tube

25.4 mm

Show Material materials with Diameter of 25.4 mm

Billet

125 mm

Show Material materials with Diameter of 125 mm

Billet

130 mm

Show Material materials with Diameter of 130 mm

Tube

Length

1000 mm

Show Material materials with Length of 1000 mm

Tube

5000 mm

Show Material materials with Length of 5000 mm

Tube

Wall thickness

0.5 - 9.0 mm

Show Material materials with Wall thickness of 0.5 - 9.0 mm

Tube

2.5 - 21.0 mm

Show Material materials with Wall thickness of 2.5 - 21.0 mm

Billet

Mechanical

PropertyValueShapeComment

Elastic modulus

100.0 - 120.0 GPa

Show Material materials with Elastic modulus of 100.0 - 120.0 GPa

Typical for Low Alloy Titanium

Elongation

15.0 - 25.0 %

Show Material materials with Elongation of 15.0 - 25.0 %

Tube

Tensile strength

480.0 - 680.0 MPa

Show Material materials with Tensile strength of 480.0 - 680.0 MPa

Tube

Thermal

PropertyValueComment

Coefficient of thermal expansion

7.599999999999997e-06 - 9.9e-06 1/K

Show Material materials with Coefficient of thermal expansion of 7.599999999999997e-06 - 9.9e-06 1/K

Typical for Low Alloy Titanium

Melting point

1650.0 - 1705.0 °C

Show Material materials with Melting point of 1650.0 - 1705.0 °C

Typical for Low Alloy Titanium

Specific heat capacity

515.0 - 597.0 J/(kg·K)

Show Material materials with Specific heat capacity of 515.0 - 597.0 J/(kg·K)

Typical for Low Alloy Titanium

Thermal conductivity

15.0 - 22.0 W/(m·K)

Show Material materials with Thermal conductivity of 15.0 - 22.0 W/(m·K)

Typical for Low Alloy Titanium

Chemical properties

PropertyValueShape

Aluminium

0.2 - 0.7 %

Show Material materials with Aluminium of 0.2 - 0.7 %

Billet, Tube

Carbon

0.07

Show Material materials with Carbon of 0.07

Billet, Tube

Nitrogen

0.04

Show Material materials with Nitrogen of 0.04

Billet, Tube

Oxygen

0.12

Show Material materials with Oxygen of 0.12

Billet, Tube

Silicon

0.1

Show Material materials with Silicon of 0.1

Billet, Tube

Zirconium

0.3

Show Material materials with Zirconium of 0.3

Billet, Tube