General
Property | Value | Related Standards | Shape |
---|---|---|---|
Density | 4.505 g/cm³ Show Material materials with Density of 4.505 g/cm³ | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Dimension
Property | Value | Related Standards | Shape |
---|---|---|---|
Diameter | 5 mm Show Material materials with Diameter of 5 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
25.4 mm Show Material materials with Diameter of 25.4 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
125 mm Show Material materials with Diameter of 125 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
130 mm Show Material materials with Diameter of 130 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | |
Length | 1000 mm Show Material materials with Length of 1000 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
5000 mm Show Material materials with Length of 5000 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube | |
Wall thickness | 0.5 - 9.0 mm Show Material materials with Wall thickness of 0.5 - 9.0 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Tube |
2.5 - 21.0 mm Show Material materials with Wall thickness of 2.5 - 21.0 mm | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Mechanical
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Elastic modulus | 120.0 GPa Show Material materials with Elastic modulus of 120.0 GPa | Typical for Pure Titanium | ||
Elongation | 11.0 - 30.0 % Show Material materials with Elongation of 11.0 - 30.0 % | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet | |
Poisson's ratio | 0.361 [-] Show Material materials with Poisson's ratio of 0.361 [-] | Typical for Pure Titanium | ||
Shear modulus | 46.0 GPa Show Material materials with Shear modulus of 46.0 GPa | Typical for Pure Titanium | ||
Tensile strength | 265.0 - 490.0 MPa Show Material materials with Tensile strength of 265.0 - 490.0 MPa | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet |
Thermal
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 8.400000000000001e-06 - 8.599999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 8.400000000000001e-06 - 8.599999999999999e-06 1/K | Typical for Pure Titanium | |||
Melting point | 1670.0 °C Show Material materials with Melting point of 1670.0 °C | Typical for Pure Titanium | |||
Specific heat capacity | 100 °C | 540 J/(kg·K) Show Material materials with Specific heat capacity of 540 J/(kg·K) | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube | |
Thermal conductivity | 18.85 W/(m·K) Show Material materials with Thermal conductivity of 18.85 W/(m·K) | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Carbon | 0.05 Show Material materials with Carbon of 0.05 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Hydrogen | 0.008 Show Material materials with Hydrogen of 0.008 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Iron | 0.15 Show Material materials with Iron of 0.15 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Nitrogen | 0.04 Show Material materials with Nitrogen of 0.04 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Oxygen | 0.1 Show Material materials with Oxygen of 0.1 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |
Silicon | 0.08 Show Material materials with Silicon of 0.08 | GOST 22178, ОSТ 190218, ТU 1-92-89, ТU 1-5-356 | Billet, Tube |