EN 3.7025

Want to keep this datasheet? Save it now in your required format

Description

This reference material is available in clad products.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

4.51 g/cm³

Show Material materials with Density of 4.51 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

105.0 GPa

Show Material materials with Elastic modulus of 105.0 GPa

Poisson's ratio

0.361 [-]

Show Material materials with Poisson's ratio of 0.361 [-]

Typical for Pure Titanium

Shear modulus

46.0 GPa

Show Material materials with Shear modulus of 46.0 GPa

Typical for Pure Titanium

Tensile strength

315.0 MPa

Show Material materials with Tensile strength of 315.0 MPa

Yield strength

180.0 MPa

Show Material materials with Yield strength of 180.0 MPa

Thermal

PropertyValueComment

Coefficient of thermal expansion

8.7e-06 1/K

Show Material materials with Coefficient of thermal expansion of 8.7e-06 1/K

Melting point

1670.0 °C

Show Material materials with Melting point of 1670.0 °C

Typical for Pure Titanium

Specific heat capacity

520.0 J/(kg·K)

Show Material materials with Specific heat capacity of 520.0 J/(kg·K)

Thermal conductivity

21.8 W/(m·K)

Show Material materials with Thermal conductivity of 21.8 W/(m·K)