General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 1.78 g/cm³ Show Material materials with Density of 1.78 g/cm³ |
Mechanical
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.68E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.68E-5 1/K |
Specific heat capacity | 23.0 °C | 1040 J/(kg·K) Show Material materials with Specific heat capacity of 1040 J/(kg·K) |
Thermal conductivity | 23.0 °C | 76.9 W/(m·K) Show Material materials with Thermal conductivity of 76.9 W/(m·K) |