Unsaturated polyester Reinforced with 15% Glass Fibres and 55% Mineral Powder (UP+GF15+MD55),Type 802

Alternative and trade names
Bakelite®
Want to keep this datasheet? Save it now in your required format

Description

Polyester moulding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability and good mechanical properties.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.95 - 2.15 g/cm³

Show Material materials with Density of 1.95 - 2.15 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

11.0 - 13.0 GPa

Show Material materials with Elastic modulus of 11.0 - 13.0 GPa

Elongation

0.6 - 1.2 %

Show Material materials with Elongation of 0.6 - 1.2 %

Impact strength, Charpy notched

2.4 - 5.5 kJ/m²

Show Material materials with Impact strength, Charpy notched of 2.4 - 5.5 kJ/m²

Impact strength, Charpy unnotched

5 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 5 kJ/m²

11 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 11 kJ/m²

Tensile strength

45.0 - 65.0 MPa

Show Material materials with Tensile strength of 45.0 - 65.0 MPa

at 0.6-1.2% strain

Thermal

PropertyValueComment

Coefficient of thermal expansion

1.5e-05 - 4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.5e-05 - 4e-05 1/K

Max service temperature

210 °C

Show Material materials with Max service temperature of 210 °C

Short

170 °C

Show Material materials with Max service temperature of 170 °C

Long

Specific heat capacity

1200 J/(kg·K)

Show Material materials with Specific heat capacity of 1200 J/(kg·K)

Thermal conductivity

0.6 - 0.8 W/(m·K)

Show Material materials with Thermal conductivity of 0.6 - 0.8 W/(m·K)

Flammability

UL 94 V1-V0

Electrical

PropertyValue

Dielectric constant

3 [-]

Show Material materials with Dielectric constant of 3 [-]

7 [-]

Show Material materials with Dielectric constant of 7 [-]

Electrical resistivity

10000000000.0 - 1000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 10000000000.0 - 1000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

ignition distributor caps, distributor fingers, spark plug connectors

Fillers

15% Glass Fiber and 55% Mineral Powder

Processing methods