General
Property | Value | Temperature |
---|---|---|
Density | 1.98 - 2.28 g/cm³ Show Material materials with Density of 1.98 - 2.28 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 11 - 13 GPa Show Material materials with Elastic modulus of 11 - 13 GPa at 23.0 °C | 23.0 °C | |
Elongation | 0.6 - 1.2 % Show Material materials with Elongation of 0.6 - 1.2 % at 23.0 °C | 23.0 °C | |
Impact strength, Charpy notched | 2.4 - 7 kJ/m² Show Material materials with Impact strength, Charpy notched of 2.4 - 7 kJ/m² at 23.0 °C | 23.0 °C | |
Impact strength, Charpy unnotched | 5 - 13 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 5 - 13 kJ/m² at 23.0 °C | 23.0 °C | |
Tensile strength | 45 - 65 MPa Show Material materials with Tensile strength of 45 - 65 MPa at 23.0 °C | 23.0 °C | at 0.6-1.2% strain |
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.5E-5 - 4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 4E-5 1/K at 23.0 °C | 23.0 °C |
Flammability | UL 94 V1-V0 | |
Max service temperature, long | 170 °C Show Material materials with Max service temperature, long of 170 °C | |
Max service temperature, short | 210 °C Show Material materials with Max service temperature, short of 210 °C | |
Specific heat capacity | 1200 J/(kg·K) Show Material materials with Specific heat capacity of 1200 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 0.6 - 0.8 W/(m·K) Show Material materials with Thermal conductivity of 0.6 - 0.8 W/(m·K) at 23.0 °C | 23.0 °C |
Electrical
Property | Value | Temperature |
---|---|---|
Dielectric constant | 3 - 7 [-] Show Material materials with Dielectric constant of 3 - 7 [-] at 23.0 °C | 23.0 °C |
Electrical resistivity | 1.00E+10 - 1.00E+12 Ω·m Show Material materials with Electrical resistivity of 1.00E+10 - 1.00E+12 Ω·m at 23.0 °C | 23.0 °C |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | explosion proof switches, safety switch housings, oven knobs, lamp parts | |
Fillers | 15% Glass Fiber and 60% Mineral Powder | |
Processing methods | Injection molding, transfer molding, compression molding |