Sheet Moulding Compound, Unsaturated Polyester Reinforced with 30% Glass Fibre (SMC UP+GF30)

Want to keep this datasheet? Save it now in your required format

Description

Glass-fiber reinforced polyester engineering polymer molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.4 - 2.0 g/cm³

Show Material materials with Density of 1.4 - 2.0 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

7.0 - 11.5 GPa

Show Material materials with Elastic modulus of 7.0 - 11.5 GPa

Elongation

1.3 - 1.5 %

Show Material materials with Elongation of 1.3 - 1.5 %

Impact strength, Charpy unnotched

50 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 50 kJ/m²

90 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 90 kJ/m²

Tensile strength

50.0 - 80.0 MPa

Show Material materials with Tensile strength of 50.0 - 80.0 MPa

at 1.3-1.5% strain

Thermal

PropertyValue

Coefficient of thermal expansion

1.5e-05 - 2e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.5e-05 - 2e-05 1/K

Specific heat capacity

1100 J/(kg·K)

Show Material materials with Specific heat capacity of 1100 J/(kg·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

4.5 [-]

Show Material materials with Dielectric constant of 4.5 [-]

4.9 [-]

Show Material materials with Dielectric constant of 4.9 [-]

Electrical resistivity

10000000000 Ω·m

Show Material materials with Electrical resistivity of 10000000000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

exterior panels, exterior body panels, engine components, ex proofed housings, automotive door panels, rail exterior, arc quenching chambers

Fillers

30% Glass Fiber

Processing methods

Compression molding