Melamine-formaldehyde Reinforced with 25% Cellulose Powder and 20% Mineral Powder (MF+LD25+MD20), Type 152.7

Alternative and trade names
Melopas®
Want to keep this datasheet? Save it now in your required format

Description

Organically and inorganically filled melamine. Very good electrical properties, excellent surface hardness, good wear and very good UV-stability, very good chemical resistance,very good food stuff resistance and food safe

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.55 - 1.75 g/cm³

Show Material materials with Density of 1.55 - 1.75 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

6.5 - 10.0 GPa

Show Material materials with Elastic modulus of 6.5 - 10.0 GPa

Elongation

0.6 - 0.9 %

Show Material materials with Elongation of 0.6 - 0.9 %

Impact strength, Charpy notched

1.3 - 1.75 kJ/m²

Show Material materials with Impact strength, Charpy notched of 1.3 - 1.75 kJ/m²

Impact strength, Charpy unnotched

5 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 5 kJ/m²

12 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 12 kJ/m²

Tensile strength

50.0 - 70.0 MPa

Show Material materials with Tensile strength of 50.0 - 70.0 MPa

at 0.6-0.9% strain

Thermal

PropertyValue

Coefficient of thermal expansion

2.5e-05 - 4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.5e-05 - 4e-05 1/K

Specific heat capacity

1200 J/(kg·K)

Show Material materials with Specific heat capacity of 1200 J/(kg·K)

Thermal conductivity

0.3 - 0.45 W/(m·K)

Show Material materials with Thermal conductivity of 0.3 - 0.45 W/(m·K)

Flammability

UL 94 V0

Electrical

PropertyValue

Dielectric constant

8 [-]

Show Material materials with Dielectric constant of 8 [-]

13.5 [-]

Show Material materials with Dielectric constant of 13.5 [-]

Electrical resistivity

1000000000.0 - 10000000000.0 Ω·m

Show Material materials with Electrical resistivity of 1000000000.0 - 10000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Tableware and cutlery, ladles, spatulas

Fillers

25% Cellulose Powder and 20% Mineral Powder

Processing methods

Injection molding, compression molding