Methylene vinyl siloxane rubber (VMQ)

Alternative and trade names
Elastosil®, Silopren™
Want to keep this datasheet? Save it now in your required format

Description

The high thermal stability, high tear strength, and broad range of durometers, portfolio also includes self-lubricating, low-compression-set. high-optical-transparency materials where both the excellent physical stability and processing advantages of silicone rubber are desired

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

1.05 - 1.44 g/cm³

Show Material materials with Density of 1.05 - 1.44 g/cm³

Mechanical

PropertyValueComment

Elongation

100.0 - 900.0 %

Show Material materials with Elongation of 100.0 - 900.0 %

Tensile strength

4.0 - 11.0 MPa

Show Material materials with Tensile strength of 4.0 - 11.0 MPa

at 100-900% strain

Thermal

PropertyValue

Coefficient of thermal expansion

0.00019 - 0.000255 1/K

Show Material materials with Coefficient of thermal expansion of 0.00019 - 0.000255 1/K

Specific heat capacity

1300.0 - 1500.0 J/(kg·K)

Show Material materials with Specific heat capacity of 1300.0 - 1500.0 J/(kg·K)

Thermal conductivity

0.17 - 0.22 W/(m·K)

Show Material materials with Thermal conductivity of 0.17 - 0.22 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

2.8 [-]

Show Material materials with Dielectric constant of 2.8 [-]

3.2 [-]

Show Material materials with Dielectric constant of 3.2 [-]

Electrical resistivity

6000000000000.0 - 500000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 6000000000000.0 - 500000000000000.0 Ω·m

Optical

PropertyValue

Transparency

yes

Technological properties

Property
Application areas

Automotive gaskets, shoe insoles, O-rings

Processing methods

Injection molding, compression molding, transfer molding, extrusion, coating, thermoforming,vulcanization