Ethylene propylene diene rubber (EPDM)

Alternative and trade names
Keltan®, Nordel™, Vistalon™, Dutral®
Want to keep this datasheet? Save it now in your required format

Description

The key features are:


  • Ozone and UV resistance
  • Water and polar fluid resistance
  • Heat resistance up to 175°C
  • Low temperature flexibility
  • Elastic properties under compression
  • Excellent physical properties at high filler loadings
  • Outstanding electrical insulation
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValue

    Density

    0.85 - 1.4 g/cm³

    Show Material materials with Density of 0.85 - 1.4 g/cm³

    Mechanical

    PropertyValueComment

    Elongation

    150.0 - 800.0 %

    Show Material materials with Elongation of 150.0 - 800.0 %

    Tensile strength

    5.0 - 33.0 MPa

    Show Material materials with Tensile strength of 5.0 - 33.0 MPa

    at 150-800% strain

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    0.000165 - 0.0002 1/K

    Show Material materials with Coefficient of thermal expansion of 0.000165 - 0.0002 1/K

    Specific heat capacity

    1800.0 - 2000.0 J/(kg·K)

    Show Material materials with Specific heat capacity of 1800.0 - 2000.0 J/(kg·K)

    Thermal conductivity

    0.15 - 0.26 W/(m·K)

    Show Material materials with Thermal conductivity of 0.15 - 0.26 W/(m·K)

    Flammability

    UL 94 V2

    Electrical

    PropertyValue

    Dielectric constant

    2.35 [-]

    Show Material materials with Dielectric constant of 2.35 [-]

    Electrical resistivity

    10000000000000.0 - 1e+16 Ω·m

    Show Material materials with Electrical resistivity of 10000000000000.0 - 1e+16 Ω·m

    Optical

    PropertyValue

    Transparency

    no

    Technological properties

    Property
    Application areas

    Sealing profiles, O-rings, hoses, cable sheathing

    Processing methods

    Compression molding, extrusion, vulcanization