Fluorine silicone rubber (FVMQ)

Alternative and trade names
Elastosil®
Want to keep this datasheet? Save it now in your required format

Description

FVMQ offers excellent chemical resistance to dilute acids and alkalines, and non-polar fluids. they have high heat and oxidative stability, outstanding low temperature flexibility, and are resistant to heat, ozone and sunlight (UV). They also offer a similar wide operational temperature range, which is much wider than that of fluorocarbon rubbers.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

1.24 - 1.27 g/cm³

Show Material materials with Density of 1.24 - 1.27 g/cm³

Mechanical

PropertyValueComment

Elongation

150.0 - 450.0 %

Show Material materials with Elongation of 150.0 - 450.0 %

Tensile strength

5.0 - 10.0 MPa

Show Material materials with Tensile strength of 5.0 - 10.0 MPa

at 150-450% strain

Thermal

PropertyValue

Coefficient of thermal expansion

0.00019 - 0.000255 1/K

Show Material materials with Coefficient of thermal expansion of 0.00019 - 0.000255 1/K

Specific heat capacity

1300.0 - 1500.0 J/(kg·K)

Show Material materials with Specific heat capacity of 1300.0 - 1500.0 J/(kg·K)

Thermal conductivity

0.22 W/(m·K)

Show Material materials with Thermal conductivity of 0.22 W/(m·K)

Optical

PropertyValue

Transparency

yes

Technological properties

Property
Application areas

Membranes, aerospace fuel system components, diaphragms

Processing methods

Injection molding, vulcanization