Epoxide; Epoxy Reinforced with 30% Glass Fibers and 20% Mineral Powder (EP+GF25+MD45)

Alternative and trade names
Bakelite®
Want to keep this datasheet? Save it now in your required format

Description

Epoxy moulding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical properties, even at higher temperatures, very slight post shrinkage, increased media resistance

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.84 - 1.9 g/cm³

Show Material materials with Density of 1.84 - 1.9 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

15.0 - 17.0 GPa

Show Material materials with Elastic modulus of 15.0 - 17.0 GPa

Elongation

4 %

Show Material materials with Elongation of 4 %

Impact strength, Charpy notched

5.0 - 9.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5.0 - 9.0 kJ/m²

Impact strength, Charpy unnotched

9 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 9 kJ/m²

14 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 14 kJ/m²

Tensile strength

70.0 - 90.0 MPa

Show Material materials with Tensile strength of 70.0 - 90.0 MPa

at 4% strain

Thermal

PropertyValue

Coefficient of thermal expansion

2e-05 - 3e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2e-05 - 3e-05 1/K

Thermal conductivity

0.6 - 0.8 W/(m·K)

Show Material materials with Thermal conductivity of 0.6 - 0.8 W/(m·K)

Flammability

UL 94 V1-V0

Electrical

PropertyValue

Dielectric constant

3.5 [-]

Show Material materials with Dielectric constant of 3.5 [-]

6.5 [-]

Show Material materials with Dielectric constant of 6.5 [-]

Electrical resistivity

100000000000.0 - 1000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 100000000000.0 - 1000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Spark plug connectors, contact strips, contact bridges

Fillers

30% Glass Fiber and 20% Mineral Powder

Processing methods

Injection molding, compression molding