Liquid-crystalline polymer Reinforced with 40% Glass Fibers (LCP+GF40)

Alternative and trade names
Zenite®, Kebaflow®, TECACOMP®
Want to keep this datasheet? Save it now in your required format

Description

It is a 40% glass fiber reinforced and lubricated liquid crystal polymer for injection molding. It has excellent impact resistance and excellent heat deflection temperature.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.68 - 1.71 g/cm³

Show Material materials with Density of 1.68 - 1.71 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

12.0 - 19.0 GPa

Show Material materials with Elastic modulus of 12.0 - 19.0 GPa

Elongation

1.0 - 2.0 %

Show Material materials with Elongation of 1.0 - 2.0 %

Impact strength, Charpy notched

10.0 - 15.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10.0 - 15.0 kJ/m²

Impact strength, Charpy unnotched

25 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 25 kJ/m²

Tensile strength

130.0 - 140.0 MPa

Show Material materials with Tensile strength of 130.0 - 140.0 MPa

at 1-2% strain

Thermal

PropertyValue

Coefficient of thermal expansion

1e-06 - 6.5e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1e-06 - 6.5e-05 1/K

Flammability

UL 94 V0

Electrical

PropertyValue

Dielectric constant

3.9 [-]

Show Material materials with Dielectric constant of 3.9 [-]

4.5 [-]

Show Material materials with Dielectric constant of 4.5 [-]

Electrical resistivity

10000000000000.0 - 100000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 10000000000000.0 - 100000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Plug connectors, LED-housings, bobbins

Fillers

40% Glass Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding