Description

It is a vinyl ester resin (Bisphenol-A epoxy based/Styrene-free/Brominated/Urethane modified) with excellent resistance against many chemicals at elevated temperatures. It brings great strength & toughness. It can be used in combination with a broad variety of fibers, including glass and carbon fibers

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.11 - 1.15 g/cm³

Show Material materials with Density of 1.11 - 1.15 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

3.0 - 4.0 GPa

Show Material materials with Elastic modulus of 3.0 - 4.0 GPa

Elongation

2.0 - 7.0 %

Show Material materials with Elongation of 2.0 - 7.0 %

Impact strength, Charpy unnotched

15 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 15 kJ/m²

30 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 30 kJ/m²

Tensile strength

60.0 - 95.0 MPa

Show Material materials with Tensile strength of 60.0 - 95.0 MPa

at 2-7% strain

Thermal

PropertyValueComment

Max service temperature

100.0 - 150.0 °C

Show Material materials with Max service temperature of 100.0 - 150.0 °C

Long

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Corrosion resistance parts, tanks relining, marine and swimming pool applications

Processing methods

Compression molding