SAE HEV-2

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.3 g/cm³

Show Material materials with Density of 8.3 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

33.5 %

Show Material materials with Elongation of 33.5 %

Reduction of area

20.0 °C

36 %

Show Material materials with Reduction of area of 36 %

760.0 °C

14 %

Show Material materials with Reduction of area of 14 %

Tensile strength

20.0 °C

1030 MPa

Show Material materials with Tensile strength of 1030 MPa

650.0 °C

800 MPa

Show Material materials with Tensile strength of 800 MPa

760.0 °C

460 MPa

Show Material materials with Tensile strength of 460 MPa

Unlock all property charts

Yield strength

20.0 °C

660 MPa

Show Material materials with Yield strength of 660 MPa

650.0 °C

590 MPa

Show Material materials with Yield strength of 590 MPa

760.0 °C

460 MPa

Show Material materials with Yield strength of 460 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

760.0 °C

1.49E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.49E-5 1/K

The mentioned value is between 20°C and the mentioned temperature

Chemical properties

PropertyValue

Carbon

0.04 %

Show Material materials with Carbon of 0.04 %

Chromium

16 %

Show Material materials with Chromium of 16 %

Cobalt

0.5 %

Show Material materials with Cobalt of 0.5 %

Copper

0.1 %

Show Material materials with Copper of 0.1 %

Iron

77.98 - 100 %

Show Material materials with Iron of 77.98 - 100 %

Manganese

2.25 %

Show Material materials with Manganese of 2.25 %

Silicon

0.08 %

Show Material materials with Silicon of 0.08 %