SAE HEV-5

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8 - 8.3 g/cm³

Show Material materials with Density of 8 - 8.3 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

208 - 215 GPa

Show Material materials with Elastic modulus of 208 - 215 GPa

Elongation A5

20.0 °C

15 - 40 %

Show Material materials with Elongation A5 of 15 - 40 %

Hardness, Rockwell C

20.0 °C

32 - 38 [-]

Show Material materials with Hardness, Rockwell C of 32 - 38 [-]

Reduction of area

20.0 °C

20 - 38 %

Show Material materials with Reduction of area of 20 - 38 %

Tensile strength

20.0 °C

1050 - 1400 MPa

Show Material materials with Tensile strength of 1050 - 1400 MPa

Yield strength

20.0 °C

620 - 969 MPa

Show Material materials with Yield strength of 620 - 969 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.19E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.19E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

200.0 °C

1.26E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.26E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

300.0 °C

1.31E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.31E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

500.0 °C

1.37E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.37E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

600.0 °C

1.33E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.33E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

700.0 °C

1.45E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.45E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

1000.0 °C

1.39E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.39E-5 1/K

The mentioned values are between 20°C and the mentioned temperature

Specific heat capacity

20.0 °C

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

20.0 °C

13 W/(m·K)

Show Material materials with Thermal conductivity of 13 W/(m·K)

Chemical properties

PropertyValue

Aluminium

1 - 1.8 %

Show Material materials with Aluminium of 1 - 1.8 %

Boron

8E-3 %

Show Material materials with Boron of 8E-3 %

Carbon

0.04 - 0.1 %

Show Material materials with Carbon of 0.04 - 0.1 %

Chromium

18 - 21 %

Show Material materials with Chromium of 18 - 21 %

Copper

0.2 %

Show Material materials with Copper of 0.2 %

Iron

3 %

Show Material materials with Iron of 3 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

1 %

Show Material materials with Silicon of 1 %

Sulfur

0.015 %

Show Material materials with Sulfur of 0.015 %

Titanium

1.8 - 2.7 %

Show Material materials with Titanium of 1.8 - 2.7 %