SAE HEV-6

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.27 g/cm³

Show Material materials with Density of 8.27 g/cm³

Mechanical

PropertyTemperatureValue

Reduction of area

20.0 °C

20 %

Show Material materials with Reduction of area of 20 %

650.0 °C

12 %

Show Material materials with Reduction of area of 12 %

760.0 °C

5 %

Show Material materials with Reduction of area of 5 %

Tensile strength

20.0 °C

1230 MPa

Show Material materials with Tensile strength of 1230 MPa

650.0 °C

940 MPa

Show Material materials with Tensile strength of 940 MPa

760.0 °C

655 MPa

Show Material materials with Tensile strength of 655 MPa

Unlock all property charts

Yield strength

20.0 °C

760 MPa

Show Material materials with Yield strength of 760 MPa

650.0 °C

620 MPa

Show Material materials with Yield strength of 620 MPa

760.0 °C

480 MPa

Show Material materials with Yield strength of 480 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

760.0 °C

1.49E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.49E-5 1/K

The mentioned value is between 20°C and the mentioned temperature

Chemical properties

PropertyValue

Aluminium

1.4 %

Show Material materials with Aluminium of 1.4 %

Boron

3E-3 %

Show Material materials with Boron of 3E-3 %

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Chromium

20 %

Show Material materials with Chromium of 20 %

Cobalt

18 %

Show Material materials with Cobalt of 18 %

Iron

55.65 - 100 %

Show Material materials with Iron of 55.65 - 100 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Silicon

1.5 %

Show Material materials with Silicon of 1.5 %