SAE J775 Grade VF-5

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

8 g/cm³

Show Material materials with Density of 8 g/cm³

Typical for Cobalt Chromium Nickel Tungsten

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

9.8E-6 - 1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 9.8E-6 - 1.3E-5 1/K

Typical for Cobalt Chromium Nickel Tungsten

Melting point

1245 - 1410 °C

Show Material materials with Melting point of 1245 - 1410 °C

Typical for Cobalt Chromium Nickel Tungsten

Specific heat capacity

23.0 °C

374 - 425 J/(kg·K)

Show Material materials with Specific heat capacity of 374 - 425 J/(kg·K)

Typical for Cobalt Chromium Nickel Tungsten

Thermal conductivity

23.0 °C

6 - 14 W/(m·K)

Show Material materials with Thermal conductivity of 6 - 14 W/(m·K)

Typical for Cobalt Chromium Nickel Tungsten

Chemical properties

PropertyValue

Carbon

1.5 - 2 %

Show Material materials with Carbon of 1.5 - 2 %

Chromium

23 - 27 %

Show Material materials with Chromium of 23 - 27 %

Iron

6 %

Show Material materials with Iron of 6 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Molybdenum

1 %

Show Material materials with Molybdenum of 1 %

Nickel

20.5 - 23.5 %

Show Material materials with Nickel of 20.5 - 23.5 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.8 - 1.5 %

Show Material materials with Silicon of 0.8 - 1.5 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Tungsten

10.5 - 13.5 %

Show Material materials with Tungsten of 10.5 - 13.5 %