Properties

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1E-5 - 1.5E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.5E-5 1/K

Typical for Cobalt Chromium Tungsten

Melting point

1185 - 1385 °C

Show Material materials with Melting point of 1185 - 1385 °C

Typical for Cobalt Chromium Tungsten

Specific heat capacity

23.0 °C

418 - 421 J/(kg·K)

Show Material materials with Specific heat capacity of 418 - 421 J/(kg·K)

Typical for Cobalt Chromium Tungsten

Thermal conductivity

23.0 °C

13 - 15 W/(m·K)

Show Material materials with Thermal conductivity of 13 - 15 W/(m·K)

Typical for Cobalt Chromium Tungsten

Chemical properties

PropertyValue

Carbon

2 - 3 %

Show Material materials with Carbon of 2 - 3 %

Chromium

26 - 33 %

Show Material materials with Chromium of 26 - 33 %

Iron

6 %

Show Material materials with Iron of 6 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Molybdenum

1 %

Show Material materials with Molybdenum of 1 %

Nickel

3 %

Show Material materials with Nickel of 3 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.4 - 2 %

Show Material materials with Silicon of 0.4 - 2 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Tungsten

11 - 14 %

Show Material materials with Tungsten of 11 - 14 %