General

PropertyTemperatureValueComment

Density

23.0 °C

9 g/cm³

Show Material materials with Density of 9 g/cm³

Typical for Cobalt Superalloy

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

6E-7 - 8.7E-6 1/K

Show Material materials with Coefficient of thermal expansion of 6E-7 - 8.7E-6 1/K

Typical for Cobalt Superalloy

Chemical properties

PropertyValue

Carbon

1.1 - 1.7 %

Show Material materials with Carbon of 1.1 - 1.7 %

Chromium

26 - 33 %

Show Material materials with Chromium of 26 - 33 %

Iron

3 %

Show Material materials with Iron of 3 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Molybdenum

1 %

Show Material materials with Molybdenum of 1 %

Nickel

3 %

Show Material materials with Nickel of 3 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.4 - 2 %

Show Material materials with Silicon of 0.4 - 2 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Tungsten

7 - 9.5 %

Show Material materials with Tungsten of 7 - 9.5 %