PropertyTemperatureValue

Hardness, Rockwell C

23.0 °C

32 - 45 [-]

Show Material materials with Hardness, Rockwell C of 32 - 45 [-]

Reduction of area

23.0 °C

15 %

Show Material materials with Reduction of area of 15 %

Tensile strength

23.0 °C

1280 MPa

Show Material materials with Tensile strength of 1280 MPa

Yield strength

23.0 °C

1030 MPa

Show Material materials with Yield strength of 1030 MPa

Chemical properties

PropertyValue

Aluminium

1.2 - 1.6 %

Show Material materials with Aluminium of 1.2 - 1.6 %

Boron

0.003 - 0.01 %

Show Material materials with Boron of 0.003 - 0.01 %

Carbon

0.03 - 0.1 %

Show Material materials with Carbon of 0.03 - 0.1 %

Chromium

18 - 21 %

Show Material materials with Chromium of 18 - 21 %

Cobalt

12 - 15 %

Show Material materials with Cobalt of 12 - 15 %

Copper

0.5 %

Show Material materials with Copper of 0.5 %

Iron

2 %

Show Material materials with Iron of 2 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Molybdenum

3.5 - 5 %

Show Material materials with Molybdenum of 3.5 - 5 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.75 %

Show Material materials with Silicon of 0.75 %

Sulfur

0.03 %

Show Material materials with Sulfur of 0.03 %

Titanium

2.75 - 3.5 %

Show Material materials with Titanium of 2.75 - 3.5 %

Zirconium

0.02 - 0.12 %

Show Material materials with Zirconium of 0.02 - 0.12 %