Description

Titanium SAE XEV-J alloy is the most commercially available of all titanium alloys. It offers an excellent combination of high strength and toughness. SAE XEV-J titanium has good welding and fabrication characteristics.

Related Standards

Equivalent Materials

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

4.506 g/cm³

Show Material materials with Density of 4.506 g/cm³

Typical for Titanium

Mechanical

PropertyValueComment

Elastic modulus

100.0 - 120.0 GPa

Show Material materials with Elastic modulus of 100.0 - 120.0 GPa

Typical for Titanium Alpha Beta Alloy

Thermal

PropertyValueComment

Coefficient of thermal expansion

7.699999999999999e-06 - 1e-05 1/K

Show Material materials with Coefficient of thermal expansion of 7.699999999999999e-06 - 1e-05 1/K

Typical for Titanium Alpha Beta Alloy

Melting point

1500.0 - 1750.0 °C

Show Material materials with Melting point of 1500.0 - 1750.0 °C

Typical for Titanium Alpha Beta Alloy

Specific heat capacity

370.0 - 674.0 J/(kg·K)

Show Material materials with Specific heat capacity of 370.0 - 674.0 J/(kg·K)

Typical for Titanium Alpha Beta Alloy

Thermal conductivity

6.0 - 12.0 W/(m·K)

Show Material materials with Thermal conductivity of 6.0 - 12.0 W/(m·K)

Typical for Titanium Alpha Beta Alloy

Chemical properties

PropertyValueRelated Standards

Aluminium

5.25 - 6.75 %

Show Material materials with Aluminium of 5.25 - 6.75 %

SAE J775

Carbon

0.1

Show Material materials with Carbon of 0.1

SAE J775

Hydrogen

0.02

Show Material materials with Hydrogen of 0.02

SAE J775

Iron

0.8

Show Material materials with Iron of 0.8

SAE J775

Nitrogen

0.1

Show Material materials with Nitrogen of 0.1

SAE J775

Oxygen

0.4

Show Material materials with Oxygen of 0.4

SAE J775

Vanadium

3.35 - 4.65 %

Show Material materials with Vanadium of 3.35 - 4.65 %

SAE J775

Yttrium

0.005

Show Material materials with Yttrium of 0.005

SAE J775