General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 3.2 g/cm³ Show Material materials with Density of 3.2 g/cm³ | Typical for Ferrosilicon |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 1250 GPa Show Material materials with Elastic modulus of 1250 GPa | Typical for Ferrosilicon |
Thermal
Property | Value | Comment |
---|---|---|
Melting point | 1200 °C Show Material materials with Melting point of 1200 °C | Typical for Ferrosilicon |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 % Show Material materials with Aluminium of 0.5 % |
Carbon | 0.1 % Show Material materials with Carbon of 0.1 % |
Manganese | 0.4 % Show Material materials with Manganese of 0.4 % |
Phosphorus | 0.04 % Show Material materials with Phosphorus of 0.04 % |
Silicon | 74 - 79 % Show Material materials with Silicon of 74 - 79 % |
Sulfur | 0.025 % Show Material materials with Sulfur of 0.025 % |