The material NiCr20AlSi with the material number 2. 4872 is applied in the form of strips and wires (see also heating conductor alloys according to DIN 17470 or electrical resistance alloys according to DIN 17471) for heating conductors and resistors. The material possesses a high electric resistance. A determinate low temperature coefficient can be adjusted, it shows a low thermoelectric potential against copper, shows a high strength and is not ferro-magnetic. The alloy is highly creep-resistant and scale-resistant. Application particularly for high-ohm resistors for measuring purposes and precision resistors.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8 g/cm³

Show Material materials with Density of 8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

150 - 245 GPa

Show Material materials with Elastic modulus of 150 - 245 GPa

Typical for Nickel Chromium Alloy

Elongation A100

20.0 °C

8 - 25 %

Show Material materials with Elongation A100 of 8 - 25 %

Tensile strength

20.0 °C

1000 MPa

Show Material materials with Tensile strength of 1000 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

7.6E-6 - 1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 7.6E-6 - 1.7E-5 1/K

Typical for Nickel Chromium Alloy

Melting point

1400 °C

Show Material materials with Melting point of 1400 °C

Typical for Nickel Chromium Alloy

Specific heat capacity

20.0 °C

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

20.0 °C

14 W/(m·K)

Show Material materials with Thermal conductivity of 14 W/(m·K)

Chemical properties

PropertyValue

Aluminium

2.5 - 4 %

Show Material materials with Aluminium of 2.5 - 4 %

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Chromium

19 - 21 %

Show Material materials with Chromium of 19 - 21 %

Copper

0.15 %

Show Material materials with Copper of 0.15 %

Iron

1 %

Show Material materials with Iron of 1 %

Manganese

0.7 %

Show Material materials with Manganese of 0.7 %

Nickel

73 %

Show Material materials with Nickel of 73 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Silicon

0.5 - 2 %

Show Material materials with Silicon of 0.5 - 2 %

Sulfur

0.015 %