Description

The expansion material NiFe47Cr with the material number 2.4486 is an alloy with controlled thermal expansion and possesses a relatively low thermal expansion up to approximately 450 °C. (Temperature interval RT to 400 °C: coefficient of thermal expansion 10.0 to 10.8 10^-6 K^-1). Its expansion properties largely correspond to those of soft glass of the lead lime or sodium lime type up to the annealing temperature. Application for sealings in soft glasses, especially lead glasses, particularly for anode cavity caps in cathode-ray television tubes. The alloy is of relatively good durability at normal temperatures in air with normal weather conditions as well as in fresh water and sea water. Application as welding filler material, too. The material is well weldable by using the tungsten inert-gas method.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.2 g/cm³

Show Material materials with Density of 8.2 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

170 GPa

Show Material materials with Elastic modulus of 170 GPa

Elongation

20.0 °C

3 - 35 %

Show Material materials with Elongation of 3 - 35 %

Hardness, Brinell

20.0 °C

120 - 280 [-]

Show Material materials with Hardness, Brinell of 120 - 280 [-]

Poisson's ratio

23.0 °C

0.28 [-]

Show Material materials with Poisson's ratio of 0.28 [-]

Typical for Nickel Iron Alloy

Tensile strength

20.0 °C

510 - 950 MPa

Show Material materials with Tensile strength of 510 - 950 MPa

Yield strength Rp0.2

20.0 °C

200 - 930 MPa

Show Material materials with Yield strength Rp0.2 of 200 - 930 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

9.1E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.1E-6 1/K

200.0 °C

9.1E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.1E-6 1/K

300.0 °C

9.1E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.1E-6 1/K

350.0 °C

9.5E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9.5E-6 1/K

400.0 °C

1.03E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.03E-5 1/K

450.0 °C

1.1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.1E-5 1/K

500.0 °C

1.15E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.15E-5 1/K

600.0 °C

1.22E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.22E-5 1/K

Melting point

1450 °C

Show Material materials with Melting point of 1450 °C

Typical for Nickel Iron Alloy

Specific heat capacity

20.0 °C

500 J/(kg·K)

Show Material materials with Specific heat capacity of 500 J/(kg·K)

Thermal conductivity

20.0 °C

14 W/(m·K)

Show Material materials with Thermal conductivity of 14 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

9.2E-7 Ω·m

Show Material materials with Electrical resistivity of 9.2E-7 Ω·m

Chemical properties

PropertyValue

Carbon

0.02 %

Show Material materials with Carbon of 0.02 %

Chromium

5.5 - 6.5 %

Show Material materials with Chromium of 5.5 - 6.5 %

Iron

44.5 - 47 %

Show Material materials with Iron of 44.5 - 47 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

45.18 %

Show Material materials with Nickel of 45.18 %

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %