DIN 1704 Grade Sn 99.75

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7.28 g/cm³

Show Material materials with Density of 7.28 g/cm³

Typical for Pure/Low Alloyed Tin

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.1E-5 - 2.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.1E-5 - 2.9E-5 1/K

Typical for Pure/Low Alloyed Tin

Melting point

232 °C

Show Material materials with Melting point of 232 °C

Typical for Pure/Low Alloyed Tin

Specific heat capacity

23.0 °C

205 - 238 J/(kg·K)

Show Material materials with Specific heat capacity of 205 - 238 J/(kg·K)

Typical for Pure/Low Alloyed Tin

Thermal conductivity

23.0 °C

52 - 74 W/(m·K)

Show Material materials with Thermal conductivity of 52 - 74 W/(m·K)

Typical for Pure/Low Alloyed Tin

Chemical properties

PropertyValue

Tin

99.75 %

Show Material materials with Tin of 99.75 %