DIN 17810 Tin alloy 1

Want to keep this datasheet? Save it now in your required format

Description

Tin alloy for the use in the manufacture of pewterware.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Thermal

PropertyTemperatureValueComment

Melting point

215 - 350 °C

Show Material materials with Melting point of 215 - 350 °C

Typical for Tin Antimony

Thermal conductivity

23.0 °C

40 W/(m·K)

Show Material materials with Thermal conductivity of 40 W/(m·K)

Typical for Tin Antimony

Chemical properties

PropertyValue

Antimony

5 - 7 %

Show Material materials with Antimony of 5 - 7 %

Bismuth

0.5 %

Show Material materials with Bismuth of 0.5 %

Cadmium

0.05 %

Show Material materials with Cadmium of 0.05 %

Copper

1 - 2.5 %

Show Material materials with Copper of 1 - 2.5 %

Lead

0.25 %

Show Material materials with Lead of 0.25 %

Silver

4 %

Show Material materials with Silver of 4 %

Tin

91 %

Show Material materials with Tin of 91 %