EN 1179 Grade Zn97.5

Want to keep this datasheet? Save it now in your required format

Description

The industrial zinc material Zn97,5, material number 2.2095, is used for zincing, for zinc sheets and strips and for alloy additives.

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.18 g/cm³

Show Material materials with Density of 7.18 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

105 GPa

Show Material materials with Elastic modulus of 105 GPa

Typical for Zinc

Poisson's ratio

23.0 °C

0.25 [-]

Show Material materials with Poisson's ratio of 0.25 [-]

Typical for Zinc

Shear modulus

23.0 °C

42 GPa

Show Material materials with Shear modulus of 42 GPa

Typical for Zinc

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.2E-5 - 2.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.8E-5 1/K

Typical for Zinc

Melting point

380 - 420 °C

Show Material materials with Melting point of 380 - 420 °C

Typical for Zinc

Specific heat capacity

23.0 °C

272 - 525 J/(kg·K)

Show Material materials with Specific heat capacity of 272 - 525 J/(kg·K)

Typical for Zinc

Thermal conductivity

23.0 °C

105 - 125 W/(m·K)

Show Material materials with Thermal conductivity of 105 - 125 W/(m·K)

Typical for Zinc

Chemical properties

PropertyValue

Cadmium

0.3 %

Show Material materials with Cadmium of 0.3 %

Iron

0.08 %

Show Material materials with Iron of 0.08 %

Lead

2.4 %

Show Material materials with Lead of 2.4 %

Zinc

97.5 %