General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 9.6 g/cm³ Show Material materials with Density of 9.6 g/cm³ | Typical for Lead Antimony |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 235 - 305 °C Show Material materials with Melting point of 235 - 305 °C | Typical for Lead Antimony | |
Specific heat capacity | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Specific heat capacity of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Thermal conductivity | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Thermal conductivity of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimony | 14 - 15.5 % Show Material materials with Antimony of 14 - 15.5 % |
Arsenic | 0.75 - 1.25 % Show Material materials with Arsenic of 0.75 - 1.25 % |
Copper | 0.1 - 0.5 % Show Material materials with Copper of 0.1 - 0.5 % |
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Lead | 81.38 % Show Material materials with Lead of 81.38 % |
Tin | 0.8 - 1.2 % Show Material materials with Tin of 0.8 - 1.2 % |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % |