General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.75 - 8.65 g/cm³ Show Material materials with Density of 7.75 - 8.65 g/cm³ | Typical for Nickel Chromium Alloy |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 150 - 245 GPa Show Material materials with Elastic modulus of 150 - 245 GPa | Typical for Nickel Chromium Alloy |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coefficient of thermal expansion of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Alloy |
Melting point | 1400 °C Show Material materials with Melting point of 1400 °C | Typical for Nickel Chromium Alloy | |
Specific heat capacity | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Specific heat capacity of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Alloy |
Thermal conductivity | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Thermal conductivity of 8 - 35 W/(m·K) | Typical for Nickel Chromium Alloy |
Chemical properties
Property | Value |
---|---|
Boron | 2.75 - 3.5 % Show Material materials with Boron of 2.75 - 3.5 % |
Chromium | 6 - 8 % Show Material materials with Chromium of 6 - 8 % |
Iron | 2 - 4 % Show Material materials with Iron of 2 - 4 % |
Nickel | 81.45 - 89.25 % Show Material materials with Nickel of 81.45 - 89.25 % |
Silicon | 3.05 % Show Material materials with Silicon of 3.05 % |