General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 5 g/cm³ Show Material materials with Density of 5 g/cm³ | Typical for Zinc Aluminium |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Poisson's ratio | 23.0 °C | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Zinc Aluminium |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.2E-5 - 2.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.2E-5 - 2.8E-5 1/K | Typical for Zinc Aluminium |
Melting point | 375 - 485 °C Show Material materials with Melting point of 375 - 485 °C | Typical for Zinc Aluminium | |
Specific heat capacity | 23.0 °C | 393 - 525 J/(kg·K) Show Material materials with Specific heat capacity of 393 - 525 J/(kg·K) | Typical for Zinc Aluminium |
Thermal conductivity | 23.0 °C | 105 - 125 W/(m·K) Show Material materials with Thermal conductivity of 105 - 125 W/(m·K) | Typical for Zinc Aluminium |
Chemical properties
Property | Value |
---|---|
Aluminium | 3.5 - 4.3 % Show Material materials with Aluminium of 3.5 - 4.3 % |
Cadmium | 4E-3 % Show Material materials with Cadmium of 4E-3 % |
Copper | 0.25 % Show Material materials with Copper of 0.25 % |
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Lead | 5E-3 % Show Material materials with Lead of 5E-3 % |
Magnesium | 0.02 - 0.06 % Show Material materials with Magnesium of 0.02 - 0.06 % |
Tin | 3E-3 % Show Material materials with Tin of 3E-3 % |
Zinc | 95.28 - 96.48 % Show Material materials with Zinc of 95.28 - 96.48 % |