SAE J473a Grade 6A

Want to keep this datasheet? Save it now in your required format

Description

Generally for joining steel and copper base alloys, Class A only for galvanized steel or zinc. Lead-tin solders are not recommended for joining aluminium, magnesium, or stainless steel.

Related Standards

This material data has been provided by SAE.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Thermal

PropertyTemperatureValueComment

Melting point

185 - 320 °C

Show Material materials with Melting point of 185 - 320 °C

Typical for Lead Tin

Specific heat capacity

23.0 °C

213 - 239 J/(kg·K)

Show Material materials with Specific heat capacity of 213 - 239 J/(kg·K)

Typical for Lead Tin

Thermal conductivity

23.0 °C

35 - 57 W/(m·K)

Show Material materials with Thermal conductivity of 35 - 57 W/(m·K)

Typical for Lead Tin

Chemical properties

PropertyValueComment

Aluminium

5E-3 %

Show Material materials with Aluminium of 5E-3 %

Antimony

0.4 %

Show Material materials with Antimony of 0.4 %

Bismuth

0.25 %

Show Material materials with Bismuth of 0.25 %

Copper

0.08 %

Show Material materials with Copper of 0.08 %

In dipping solders, 0.5% max copper is permissible

Iron

0.02 %

Show Material materials with Iron of 0.02 %

Tin

14 - 15 %

Show Material materials with Tin of 14 - 15 %

Zinc

5E-3 %

Show Material materials with Zinc of 5E-3 %