PropertyValue

Manganese

85 - 90 %

Show Material materials with Manganese of 85 - 90 %

Phosphorus

0.2 %

Show Material materials with Phosphorus of 0.2 %

Silicon

2 %

Show Material materials with Silicon of 2 %

Sulfur

0.02 %

Show Material materials with Sulfur of 0.02 %