General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.7 g/cm³ Show Material materials with Density of 7.7 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 154 - 190 GPa Show Material materials with Elastic modulus of 154 - 190 GPa | |
Hardness, Vickers | 20.0 °C | 420 [-] Show Material materials with Hardness, Vickers of 420 [-] | |
Poisson's ratio | 23.0 °C | 0.27 [-] Show Material materials with Poisson's ratio of 0.27 [-] | Typical for Cast Iron |
Shear modulus | 23.0 °C | 41 GPa Show Material materials with Shear modulus of 41 GPa | Typical for Cast Iron |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 1/K | Typical for White Cast Iron |
Melting point | 1209 °C Show Material materials with Melting point of 1209 °C | Typical for White Cast Iron | |
Specific heat capacity | 23.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | Typical for White Cast Iron |
Thermal conductivity | 20.0 °C | 13.8 W/(m·K) Show Material materials with Thermal conductivity of 13.8 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbon | 2.3 - 2.9 % Show Material materials with Carbon of 2.3 - 2.9 % |
Chromium | 18 - 22 % Show Material materials with Chromium of 18 - 22 % |
Manganese | 0.5 - 1 % Show Material materials with Manganese of 0.5 - 1 % |
Molybdenum | 1.4 - 2 % Show Material materials with Molybdenum of 1.4 - 2 % |
Nickel | 0.8 - 1.2 % Show Material materials with Nickel of 0.8 - 1.2 % |
Silicon | 0.2 - 0.8 % Show Material materials with Silicon of 0.2 - 0.8 % |