DIN 17405 Grade RSi12

Want to keep this datasheet? Save it now in your required format

Description

Application: continuous current relais and the like Former material number: 1.3845

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 - 210 GPa

Show Material materials with Elastic modulus of 190 - 210 GPa

Typical for Soft Magnetic Iron

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2E-6 - 1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2E-6 - 1.2E-5 1/K

Typical for Soft Magnetic Iron

Specific heat capacity

23.0 °C

470 J/(kg·K)

Show Material materials with Specific heat capacity of 470 J/(kg·K)

Typical for Soft Magnetic Iron

Thermal conductivity

23.0 °C

13 - 55 W/(m·K)

Show Material materials with Thermal conductivity of 13 - 55 W/(m·K)

Typical for Soft Magnetic Iron

Technological properties

Property
Features

Soft magnetic