General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 8.3 g/cm³ Show Material materials with Density of 8.3 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 152 GPa Show Material materials with Elastic modulus of 152 GPa |
Elongation | 20.0 °C | 12 % Show Material materials with Elongation of 12 % |
Hardness, Brinell | 20.0 °C | 80 [-] Show Material materials with Hardness, Brinell of 80 [-] |
Tensile strength | 20.0 °C | 320 MPa Show Material materials with Tensile strength of 320 MPa |
Yield strength Rp0.2 | 20.0 °C | 120 MPa Show Material materials with Yield strength Rp0.2 of 120 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 8.5E-6 - 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 8.5E-6 - 1.4E-5 1/K | Typical for Pure/Low Nickel Alloy |
Melting point | 1400 - 1500 °C Show Material materials with Melting point of 1400 - 1500 °C | Typical for Pure/Low Nickel Alloy | |
Specific heat capacity | 23.0 °C | 430 - 532 J/(kg·K) Show Material materials with Specific heat capacity of 430 - 532 J/(kg·K) | Typical for Pure/Low Nickel Alloy |
Thermal conductivity | 23.0 °C | 18 - 86 W/(m·K) Show Material materials with Thermal conductivity of 18 - 86 W/(m·K) | Typical for Pure/Low Nickel Alloy |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 20.0 °C | 2.85E-7 Ω·m Show Material materials with Electrical resistivity of 2.85E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbon | 1 % Show Material materials with Carbon of 1 % |
Copper | 1.2 % Show Material materials with Copper of 1.2 % |
Iron | 1 % Show Material materials with Iron of 1 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Nickel | 95 % Show Material materials with Nickel of 95 % |
Silicon | 2 % Show Material materials with Silicon of 2 % |
Technological properties
Property | ||
---|---|---|
Processing methods | sand casting, separately cast test sample |