General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 8.6 g/cm³ Show Material materials with Density of 8.6 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 120 - 156 GPa Show Material materials with Elastic modulus of 120 - 156 GPa | Typical for Nickel Copper Alloy |
Elongation | 20.0 °C | 25 % Show Material materials with Elongation of 25 % | |
Hardness, Brinell | 20.0 °C | 120 [-] Show Material materials with Hardness, Brinell of 120 [-] | |
Tensile strength | 20.0 °C | 450 MPa Show Material materials with Tensile strength of 450 MPa | |
Yield strength Rp0.2 | 20.0 °C | 220 MPa Show Material materials with Yield strength Rp0.2 of 220 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.1E-5 - 1.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 - 1.6E-5 1/K | Typical for Nickel Copper Alloy |
Melting point | 1170 - 1365 °C Show Material materials with Melting point of 1170 - 1365 °C | Typical for Nickel Copper Alloy | |
Specific heat capacity | 23.0 °C | 418 - 540 J/(kg·K) Show Material materials with Specific heat capacity of 418 - 540 J/(kg·K) | Typical for Nickel Copper Alloy |
Thermal conductivity | 23.0 °C | 16 - 45 W/(m·K) Show Material materials with Thermal conductivity of 16 - 45 W/(m·K) | Typical for Nickel Copper Alloy |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 % Show Material materials with Aluminium of 0.5 % |
Carbon | 0.15 % Show Material materials with Carbon of 0.15 % |
Copper | 26 - 33 % Show Material materials with Copper of 26 - 33 % |
Iron | 1 - 2.5 % Show Material materials with Iron of 1 - 2.5 % |
Lead | 0.01 % Show Material materials with Lead of 0.01 % |
Magnesium | 0.12 % Show Material materials with Magnesium of 0.12 % |
Manganese | 0.5 - 1.5 % Show Material materials with Manganese of 0.5 - 1.5 % |
Nickel | 62 - 68 % Show Material materials with Nickel of 62 - 68 % |
Niobium | 1 - 1.5 % Show Material materials with Niobium of 1 - 1.5 % |
Silicon | 0.5 - 1.5 % Show Material materials with Silicon of 0.5 - 1.5 % |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % |
Titanium | 0.2 % Show Material materials with Titanium of 0.2 % |
Technological properties
Property | ||
---|---|---|
Processing methods | sand casting, separately cast test sample |