General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.2 - 7.34 g/cm³ Show Material materials with Density of 7.2 - 7.34 g/cm³ | Typical for Malleable Cast Iron |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 179 GPa Show Material materials with Elastic modulus of 179 GPa | |
Elongation | 23.0 °C | 3 % Show Material materials with Elongation of 3 % | |
Hardness, Brinell | 23.0 °C | 187 - 241 [-] Show Material materials with Hardness, Brinell of 187 - 241 [-] | |
Poisson's ratio | 23.0 °C | 0.27 [-] Show Material materials with Poisson's ratio of 0.27 [-] | Typical for Malleable Cast Iron |
Shear modulus | 23.0 °C | 64 GPa Show Material materials with Shear modulus of 64 GPa | Typical for Malleable Cast Iron |
Tensile strength | 23.0 °C | 517 MPa Show Material materials with Tensile strength of 517 MPa | |
Yield strength | 23.0 °C | 379 MPa Show Material materials with Yield strength of 379 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1E-5 - 1.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 1.4E-5 1/K | Typical for Malleable Cast Iron |
Melting point | 1120 °C Show Material materials with Melting point of 1120 °C | Typical for Cast Iron | |
Specific heat capacity | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Specific heat capacity of 460 - 527 J/(kg·K) | Typical for Malleable Cast Iron |
Thermal conductivity | 23.0 °C | 51 W/(m·K) Show Material materials with Thermal conductivity of 51 W/(m·K) | Typical for Malleable Cast Iron |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbon | 2.2 - 2.9 % Show Material materials with Carbon of 2.2 - 2.9 % | |
Iron | 93.6 - 96.71 % Show Material materials with Iron of 93.6 - 96.71 % | balance |
Manganese | 0.15 - 1.25 % Show Material materials with Manganese of 0.15 - 1.25 % | |
Phosphorus | 0.02 - 0.1 % Show Material materials with Phosphorus of 0.02 - 0.1 % | |
Silicon | 0.9 - 1.9 % Show Material materials with Silicon of 0.9 - 1.9 % | |
Sulfur | 0.02 - 0.2 % Show Material materials with Sulfur of 0.02 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Parts requiring moderate strength. | |
Processing history | as agreed |