General
Property | Value | Comment |
---|---|---|
Density | 2.65 - 2.71 g/cm³ Show Material materials with Density of 2.65 - 2.71 g/cm³ | Typical for Cast 4xx.x Series Aluminium |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 71.0 - 75.0 GPa Show Material materials with Elastic modulus of 71.0 - 75.0 GPa | Typical for Cast 4xx.x Series Aluminium | |||
Hardness, Brinell | 40.0 [-] Show Material materials with Hardness, Brinell of 40.0 [-] | F | ASTM B26 | Casting | |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 4xx.x Series Aluminium | |||
Tensile strength | 115.0 MPa Show Material materials with Tensile strength of 115.0 MPa | F | ASTM B26 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2e-05 - 2.2e-05 1/K Show Material materials with Coefficient of thermal expansion of 2e-05 - 2.2e-05 1/K | Typical for Cast 4xx.x Series Aluminium |
Melting point | 565.0 - 630.0 °C Show Material materials with Melting point of 565.0 - 630.0 °C | Typical for Cast 4xx.x Series Aluminium |
Specific heat capacity | 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 963.0 J/(kg·K) | Typical for Cast 4xx.x Series Aluminium |
Thermal conductivity | 130.0 - 170.0 W/(m·K) Show Material materials with Thermal conductivity of 130.0 - 170.0 W/(m·K) | Typical for Cast 4xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Copper | 0.15 Show Material materials with Copper of 0.15 | F | ASTM B26 | Casting |
Iron | 0.8 Show Material materials with Iron of 0.8 | F | ASTM B26 | Casting |
Magnesium | 0.05 Show Material materials with Magnesium of 0.05 | F | ASTM B26 | Casting |
Manganese | 0.35 Show Material materials with Manganese of 0.35 | F | ASTM B26 | Casting |
Silicon | 4.5 - 6.0 % Show Material materials with Silicon of 4.5 - 6.0 % | F | ASTM B26 | Casting |
Titanium | 0.25 Show Material materials with Titanium of 0.25 | F | ASTM B26 | Casting |
Zinc | 0.35 Show Material materials with Zinc of 0.35 | F | ASTM B26 | Casting |