General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7 g/cm³ Show Material materials with Density of 7 g/cm³ | Typical for Cast/Wrought Aluminium Zinc Grade |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 40 - 45 GPa Show Material materials with Elastic modulus of 40 - 45 GPa | Typical for Cast/Wrought Aluminium Zinc Grade |
Elongation A50 | 23.0 °C | 2 % Show Material materials with Elongation A50 of 2 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Magnesium |
Shear modulus | 23.0 °C | 45 GPa Show Material materials with Shear modulus of 45 GPa | Typical for Magnesium |
Tensile strength | 23.0 °C | 158 MPa Show Material materials with Tensile strength of 158 MPa | |
Yield strength Rp0.2 | 23.0 °C | 83 MPa Show Material materials with Yield strength Rp0.2 of 83 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.5E-5 - 2.6E-5 1/K | Typical for Cast/Wrought Aluminium Zinc Grade |
Melting point | 365 - 645 °C Show Material materials with Melting point of 365 - 645 °C | Typical for Cast/Wrought Aluminium Zinc Grade | |
Specific heat capacity | 23.0 °C | 800 - 1100 J/(kg·K) Show Material materials with Specific heat capacity of 800 - 1100 J/(kg·K) | Typical for Cast/Wrought Aluminium Zinc Grade |
Thermal conductivity | 23.0 °C | 44 - 110 W/(m·K) Show Material materials with Thermal conductivity of 44 - 110 W/(m·K) | Typical for Cast/Wrought Aluminium Zinc Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 8.1 - 9.3 % Show Material materials with Aluminium of 8.1 - 9.3 % |
Copper | 0.1 % Show Material materials with Copper of 0.1 % |
Manganese | 0.13 - 0.35 % Show Material materials with Manganese of 0.13 - 0.35 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Silicon | 0.3 % Show Material materials with Silicon of 0.3 % |
Zinc | 0.4 - 1 % Show Material materials with Zinc of 0.4 - 1 % |