ASTM AZ92A F

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

7 g/cm³

Show Material materials with Density of 7 g/cm³

Typical for Cast/Wrought Aluminium Zinc Grade

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

40 - 45 GPa

Show Material materials with Elastic modulus of 40 - 45 GPa

Typical for Cast/Wrought Aluminium Zinc Grade

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for Magnesium

Shear modulus

23.0 °C

45 GPa

Show Material materials with Shear modulus of 45 GPa

Typical for Magnesium

Tensile strength

23.0 °C

158 MPa

Show Material materials with Tensile strength of 158 MPa

Yield strength Rp0.2

23.0 °C

76 MPa

Show Material materials with Yield strength Rp0.2 of 76 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.5E-5 - 2.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.5E-5 - 2.6E-5 1/K

Typical for Cast/Wrought Aluminium Zinc Grade

Melting point

365 - 645 °C

Show Material materials with Melting point of 365 - 645 °C

Typical for Cast/Wrought Aluminium Zinc Grade

Specific heat capacity

23.0 °C

800 - 1100 J/(kg·K)

Show Material materials with Specific heat capacity of 800 - 1100 J/(kg·K)

Typical for Cast/Wrought Aluminium Zinc Grade

Thermal conductivity

23.0 °C

44 - 110 W/(m·K)

Show Material materials with Thermal conductivity of 44 - 110 W/(m·K)

Typical for Cast/Wrought Aluminium Zinc Grade

Chemical properties

PropertyValue

Aluminium

8.3 - 9.7 %

Show Material materials with Aluminium of 8.3 - 9.7 %

Copper

0.25 %

Show Material materials with Copper of 0.25 %

Manganese

0.1 - 0.35 %

Show Material materials with Manganese of 0.1 - 0.35 %

Nickel

0.01 %

Show Material materials with Nickel of 0.01 %

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %

Zinc

1.6 - 2.4 %

Show Material materials with Zinc of 1.6 - 2.4 %