General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.7 g/cm³ Show Material materials with Density of 1.7 g/cm³ | Typical for Cast Rare Earth Grade |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 40 - 45 GPa Show Material materials with Elastic modulus of 40 - 45 GPa | Typical for Cast Rare Earth Grade |
Elongation A50 | 23.0 °C | 2 % Show Material materials with Elongation A50 of 2 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Magnesium |
Shear modulus | 23.0 °C | 45 GPa Show Material materials with Shear modulus of 45 GPa | Typical for Magnesium |
Tensile strength | 23.0 °C | 138 MPa Show Material materials with Tensile strength of 138 MPa | |
Yield strength Rp0.2 | 23.0 °C | 96 MPa Show Material materials with Yield strength Rp0.2 of 96 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.6E-5 1/K | Typical for Cast Rare Earth Grade |
Melting point | 535 - 645 °C Show Material materials with Melting point of 535 - 645 °C | Typical for Cast Rare Earth Grade | |
Specific heat capacity | 23.0 °C | 966 - 1050 J/(kg·K) Show Material materials with Specific heat capacity of 966 - 1050 J/(kg·K) | Typical for Cast Rare Earth Grade |
Thermal conductivity | 23.0 °C | 51 - 113 W/(m·K) Show Material materials with Thermal conductivity of 51 - 113 W/(m·K) | Typical for Cast Rare Earth Grade |
Chemical properties
Property | Value |
---|---|
Copper | 0.1 % Show Material materials with Copper of 0.1 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Rare Earth Elements | 2.5 - 4 % Show Material materials with Rare Earth Elements of 2.5 - 4 % |
Zinc | 2 - 3.1 % Show Material materials with Zinc of 2 - 3.1 % |
Zirconium | 0.5 - 1 % Show Material materials with Zirconium of 0.5 - 1 % |