General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.18 g/cm³ Show Material materials with Density of 7.18 g/cm³ | Typical for Wrought Zinc Grade |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 44.8 GPa Show Material materials with Elastic modulus of 44.8 GPa | |
Elongation A50 | 23.0 °C | 4 % Show Material materials with Elongation A50 of 4 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Magnesium |
Shear modulus | 23.0 °C | 45 GPa Show Material materials with Shear modulus of 45 GPa | Typical for Magnesium |
Tensile strength | 23.0 °C | 255 - 275 MPa Show Material materials with Tensile strength of 255 - 275 MPa | |
Yield strength Rp0.2 | 23.0 °C | 235 - 255 MPa Show Material materials with Yield strength Rp0.2 of 235 - 255 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.7E-5 - 2.72E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.7E-5 - 2.72E-5 1/K | Typical for Wrought Zinc Grade |
Melting point | 520 - 635 °C Show Material materials with Melting point of 520 - 635 °C | Typical for Wrought Zinc Grade | |
Specific heat capacity | 23.0 °C | 1050 J/(kg·K) Show Material materials with Specific heat capacity of 1050 J/(kg·K) | Typical for Wrought Zinc Grade |
Thermal conductivity | 23.0 °C | 117 - 146 W/(m·K) Show Material materials with Thermal conductivity of 117 - 146 W/(m·K) | Typical for Wrought Zinc Grade |
Chemical properties
Property | Value |
---|---|
Zinc | 3.5 - 4.5 % Show Material materials with Zinc of 3.5 - 4.5 % |
Zirconium | 0.45 % Show Material materials with Zirconium of 0.45 % |