General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.74 g/cm³ Show Material materials with Density of 1.74 g/cm³ | Typical for Magnesium |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 45 GPa Show Material materials with Elastic modulus of 45 GPa | Typical for Magnesium |
Elongation | 23.0 °C | 2.5 % Show Material materials with Elongation of 2.5 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | Typical for Magnesium |
Shear modulus | 23.0 °C | 45 GPa Show Material materials with Shear modulus of 45 GPa | Typical for Magnesium |
Tensile strength | 23.0 °C | 200 MPa Show Material materials with Tensile strength of 200 MPa | |
Yield strength Rp0.2 | 23.0 °C | 133 MPa Show Material materials with Yield strength Rp0.2 of 133 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.3E-5 - 2.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 - 2.6E-5 1/K | Typical for Magnesium |
Melting point | 650 °C Show Material materials with Melting point of 650 °C | Typical for Magnesium | |
Specific heat capacity | 23.0 °C | 1010 - 1060 J/(kg·K) Show Material materials with Specific heat capacity of 1010 - 1060 J/(kg·K) | Typical for Magnesium |
Thermal conductivity | 23.0 °C | 153 - 167 W/(m·K) Show Material materials with Thermal conductivity of 153 - 167 W/(m·K) | Typical for Magnesium |
Chemical properties
Property | Value |
---|---|
Copper | 0.1 % Show Material materials with Copper of 0.1 % |
Manganese | 0.15 % Show Material materials with Manganese of 0.15 % |
Nickel | 0.01 % Show Material materials with Nickel of 0.01 % |
Rare Earth Elements | 0.75 - 1.75 % Show Material materials with Rare Earth Elements of 0.75 - 1.75 % |
Zinc | 3.5 - 5 % Show Material materials with Zinc of 3.5 - 5 % |
Zirconium | 0.4 - 1 % Show Material materials with Zirconium of 0.4 - 1 % |