Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.15 g/cm³ Show Material materials with Density of 7.15 g/cm³ | Typical for Grey Cast Iron |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 92.4 GPa Show Material materials with Elastic modulus of 92.4 GPa | Typical for Grey Cast Iron |
Poisson's ratio | 23.0 °C | 0.21 [-] Show Material materials with Poisson's ratio of 0.21 [-] | Typical for Grey Cast Iron |
Shear modulus | 23.0 °C | 41 GPa Show Material materials with Shear modulus of 41 GPa | Typical for Cast Iron |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.1E-5 - 1.5E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.1E-5 - 1.5E-5 1/K | Typical for Grey Cast Iron |
Melting point | 1127 - 1204 °C Show Material materials with Melting point of 1127 - 1204 °C | Typical for Grey Cast Iron | |
Specific heat capacity | 23.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | Typical for Grey Cast Iron |
Thermal conductivity | 23.0 °C | 20 - 80 W/(m·K) Show Material materials with Thermal conductivity of 20 - 80 W/(m·K) | Typical for Grey Cast Iron |