General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.75 g/cm³ Show Material materials with Density of 7.75 g/cm³ | Typical for Iron Alloy |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Compressive yield strength | 20.0 °C | 630 - 840 MPa Show Material materials with Compressive yield strength of 630 - 840 MPa | |
Elastic modulus | 23.0 °C | 210 GPa Show Material materials with Elastic modulus of 210 GPa | Typical for Iron Alloy |
Hardness, Brinell | 20.0 °C | 120 - 150 [-] Show Material materials with Hardness, Brinell of 120 - 150 [-] | |
Poisson's ratio | 23.0 °C | 0.28 [-] Show Material materials with Poisson's ratio of 0.28 [-] | Typical for Iron Alloy |
Tensile strength | 20.0 °C | 140 - 220 MPa Show Material materials with Tensile strength of 140 - 220 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1E-5 - 2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 2E-5 1/K | Typical for Iron Alloy |
Chemical properties
Property | Value |
---|---|
Carbon | 3 % Show Material materials with Carbon of 3 % |
Chromium | 0.2 % Show Material materials with Chromium of 0.2 % |
Manganese | 6 - 7 % Show Material materials with Manganese of 6 - 7 % |
Nickel | 12 - 14 % Show Material materials with Nickel of 12 - 14 % |
Silicon | 1.5 - 3 % Show Material materials with Silicon of 1.5 - 3 % |
Do you have a technical question or need more information about this material?