Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.75 g/cm³ Show Material materials with Density of 7.75 g/cm³ | Typical for Iron Alloy |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 210 GPa Show Material materials with Elastic modulus of 210 GPa | Typical for Iron Alloy |
Elongation | 20.0 °C | 2 % Show Material materials with Elongation of 2 % | |
Hardness, Brinell | 20.0 °C | 140 - 250 [-] Show Material materials with Hardness, Brinell of 140 - 250 [-] | |
Poisson's ratio | 23.0 °C | 0.28 [-] Show Material materials with Poisson's ratio of 0.28 [-] | Typical for Iron Alloy |
Tensile strength | 20.0 °C | 190 - 280 MPa Show Material materials with Tensile strength of 190 - 280 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1E-5 - 2E-5 1/K Show Material materials with Coefficient of thermal expansion of 1E-5 - 2E-5 1/K | Typical for Iron Alloy |
Chemical properties
Property | Value |
---|---|
Carbon | 2.5 % Show Material materials with Carbon of 2.5 % |
Chromium | 1.5 - 4.5 % Show Material materials with Chromium of 1.5 - 4.5 % |
Manganese | 0.5 - 1.5 % Show Material materials with Manganese of 0.5 - 1.5 % |
Nickel | 18 - 22 % Show Material materials with Nickel of 18 - 22 % |
Silicon | 3.5 - 5.5 % Show Material materials with Silicon of 3.5 - 5.5 % |