Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.4 g/cm³ Show Material materials with Density of 7.4 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 20.0 °C | 165 - 180 GPa Show Material materials with Elastic modulus of 165 - 180 GPa | |
Hardness, Vickers | 20.0 °C | 300 [-] Show Material materials with Hardness, Vickers of 300 [-] | |
Poisson's ratio | 23.0 °C | 0.27 [-] Show Material materials with Poisson's ratio of 0.27 [-] | Typical for Cast Iron |
Shear modulus | 23.0 °C | 41 GPa Show Material materials with Shear modulus of 41 GPa | Typical for Cast Iron |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Melting point | 1120 °C Show Material materials with Melting point of 1120 °C | Typical for Cast Iron | |
Specific heat capacity | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Specific heat capacity of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Thermal conductivity | 23.0 °C | 55 W/(m·K) Show Material materials with Thermal conductivity of 55 W/(m·K) | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Carbon | 2.8 - 3.5 % Show Material materials with Carbon of 2.8 - 3.5 % |
Manganese | 0.2 - 0.5 % Show Material materials with Manganese of 0.2 - 0.5 % |
Molybdenum | 0.5 - 0.8 % Show Material materials with Molybdenum of 0.5 - 0.8 % |
Nickel | 1.5 - 4.5 % Show Material materials with Nickel of 1.5 - 4.5 % |
Silicon | 2 - 2.6 % Show Material materials with Silicon of 2 - 2.6 % |